##  <a> </a> 

#  Cracking 

 

 

 

 

  Paint Defects

  

 

      ![TST 64.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/TST%2064.png.webp?itok=mJ7bMi7W "TST 64.png")  



 

 Causes

- Faulty paint system on thermoplastic substrates
- (direct application of polyester putty or filler, wash primer, or synthetic resin products on TPA)
- Flash-off too short in wet-on-wet application

 

 

 

      ![paint defect - prevention.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/paint%20defect%20-%20prevention.png.webp?itok=lhkqUPyU "paint defect - prevention.png")  



 

 Prevention

- Respect the refinishing procedures for factory-applied TPA finishes
- Respect the recommended flash-off times between coats

 

 

 

      ![paint defects - repair.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/paint%20defects%20-%20repair_0.png.webp?itok=eXS0Aq4P "paint defects - repair.png")  



 

 How to repair

- Sand the paint film back to a sound substrate
- Repaint using suitable undercoat and finishing materials

 

 

 

 

 

 

 

 



Repair Steps

[Basecoat/ Topcoat](/en-emea/taxonomy/term/165)

[Clearcoat](/en-emea/taxonomy/term/166)

[Primer/ Filler](/en-emea/taxonomy/term/172)

[Putty](/en-emea/taxonomy/term/162)

[Sanding Filler](/en-emea/taxonomy/term/163)

[Wet-on-Wet Filler](/en-emea/taxonomy/term/164)

 

 

 

 Start working with baslac today. It just makes sense.

 

  [Contact us

  ](/en-emea/contact-us "Contact us")  

 

 

 Get in touch with your local baslac dealer now and start working smarter.

 

  [Find a dealer near you

  ](/en-emea/dealers "Find a dealer near you")