#  Loss of adhesion 

 

 

 

 

  Paint Defects

  

 

      ![TST 66.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/TST%2066.png.webp?itok=svSaMywr "TST 66.png")  



 

 Causes

- Contaminants left on the substrate, underneath the paint system (such as silicone, oil, wax, water, corrosion, etc.)
- Use of an unsuitable filler
- Use of incorrect cleaner
- Insufficient sanding of the substrate
- Undercoats too thin
- Drying time too short

 

 

 

      ![paint defect - prevention.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/paint%20defect%20-%20prevention.png.webp?itok=lhkqUPyU "paint defect - prevention.png")  



 

 Prevention

- Take greatest care to thoroughly clean all surfaces to be painted
- Make sure you use only fillers that are suitable for the substrates being painted
- Apply the individual coats correctly, and flash off between coats as specified
- Correctly sand the surfaces to be painted
- Use recommended baslac cleaners

 

 

 

      ![paint defects - repair.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/paint%20defects%20-%20repair_0.png.webp?itok=eXS0Aq4P "paint defects - repair.png")  



 

 How to repair

- Strip the paintwork from an area larger than that affected, and refinish the stripped areas all over again

 

 

 

 

 

 

 

 



Repair Steps

[Basecoat/ Topcoat](/en-emea/taxonomy/term/165)

[Clearcoat](/en-emea/taxonomy/term/166)

[Primer/ Filler](/en-emea/taxonomy/term/172)

[Putty](/en-emea/taxonomy/term/162)

[Sanding Filler](/en-emea/taxonomy/term/163)

[Wet-on-Wet Filler](/en-emea/taxonomy/term/164)

 

 

 

 Start working with baslac today. It just makes sense.

 

  [Contact us

  ](/en-emea/contact-us "Contact us")  

 

 

 Get in touch with your local baslac dealer now and start working smarter.

 

  [Find a dealer near you

  ](/en-emea/dealers "Find a dealer near you")