#  Peeling of on plastic parts 

 

 

 

 

  Paint Defects

  

 

      ![TST 68.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/TST%2068.png.webp?itok=YSaa8jLl "TST 68.png")  



 

 Causes

- Poor cleaning of the plastic substrate
- Use of an unsuitable or too little cleaning or degreasing agent
- Plastic part not heated before paint application
- No adhesion promoter used
- Plastic not paintable

 

 

 

      ![paint defect - prevention.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/paint%20defect%20-%20prevention.png.webp?itok=lhkqUPyU "paint defect - prevention.png")  



 

 Prevention

- Thoroughly clean the parts using a mild detergent
- Clean the substrate before and after every manipulation
- Use correct plastic cleaner
- Plastic parts should be heated to 60°C to force out any residual contaminants (Make sure that the panel will not lose its shape due to the heat)
- Apply plastic primer according to technical data sheet
- Control if plastic is paintable

 

 

 

      ![paint defects - repair.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/paint%20defects%20-%20repair_0.png.webp?itok=eXS0Aq4P "paint defects - repair.png")  



 

 How to repair

- Completely remove the peeling paintwork and refinish the affected areas

 

 

 

 

 

 

 

 



Repair Steps

[Basecoat/ Topcoat](/en-emea/taxonomy/term/165)

[Clearcoat](/en-emea/taxonomy/term/166)

[Primer/ Filler](/en-emea/taxonomy/term/172)

[Putty](/en-emea/taxonomy/term/162)

[Sanding Filler](/en-emea/taxonomy/term/163)

[Wet-on-Wet Filler](/en-emea/taxonomy/term/164)

 

 

 

 Start working with baslac today. It just makes sense.

 

  [Contact us

  ](/en-emea/contact-us "Contact us")  

 

 

 Get in touch with your local baslac dealer now and start working smarter.

 

  [Find a dealer near you

  ](/en-emea/dealers "Find a dealer near you")