Peeling of on plastic parts

Paint Defects

TST 68.png

Causes

  • Poor cleaning of the plastic substrate
  • Use of an unsuitable or too little cleaning or degreasing agent
  • Plastic part not heated before paint application
  • No adhesion promoter used
  • Plastic not paintable
paint defect - prevention.png

Prevention

  • Thoroughly clean the parts using a mild detergent
  • Clean the substrate before and after every manipulation
  • Use correct plastic cleaner
  • Plastic parts should be heated to 60°C to force out any residual contaminants (Make sure that the panel will not lose its shape due to the heat)
  • Apply plastic primer according to technical data sheet
  • Control if plastic is paintable
paint defects - repair.png

How to repair

  • Completely remove the peeling paintwork and refinish the affected areas