Blend into adjacent panel Non VOC 35 1. Cleaning step Clean carefully with cleaner 70-10 Use wipe on wipe off method 2. Preparation steps Tag cloth the area to be painted 3. Mixing ratio 35- Basecoat 100% 60-20/30/40 Diluter 50% temperature chart 4. Application first coat Spray gun HVLP or RP 1.3 pressure 2.0 bar Spray 1 coat on the wing Flash off 5. Cleaning Tag cloth the overspray on the door 6. Application method second coat Spray gun HVLP or RP 1.3 pressure 2.0 bar Spray second coat on wing No flash off 7. Application method Reduce pressure to 0.8 to max 1.5 bar and blend in the door Flash off 8. Mist coat Apply mist coat over repaired area Spray gun distance approx. 30 cm from object Flash off Ready for clear coat Repair Steps Teinte de base Commencez à travailler avec baslac dès aujourd’hui. Discutons Contactez votre distributeur baslac local dès maintenant. Trouvez un distributeur près de chez vous