Blend into repaired panel

VOC 45 Line

TST 24 (1).png

1. Cleaning

  • Clean carefully with cleaner 70-45
  • Use wipe on, wipe off method
TST 24 (4).png

2. Preparation steps

  • Tag cloth the area to be painted
TST 24 (3).png

3. Mixing ratio of basecoat:

TST 24 (5).png

4. 45_basecoat_1.jpg

  • Spray gun HVLP 1.4,  pressure 0.8 to 1.5 bar
  • Cover filler patch with reduced pressure until covered
  • Keep the patch as small as possible
  • Flash off until matt
TST 24 (6).png

5. Mixing blend in clear:

  • 45-W10 100%
  • 45-R45 Diluter 70%
TST 24 (2).png

6. Blend in clear

  • Spray gun HVLP 1.4 pressure 2.0
  • Spray 1 wet coat until 10 cm of edges
  • No flash off
TST 24 (9).png

7. Mixing blend in clear and basecoat

  • Mix RFU blend in clear and RFU basecoat 1:1
TST 24 (7).png

8, Blend in of base coat

  • Blend in the filler patch into wet blend-in clear
  • Spray gun HVLP 1.4 pressure 0.8 to 1.5
  • Flash off
TST 24 (8).png

9. Mist coat

  • Apply a mist coat over the repaired area
  • Spray gun distance is 30 cm
  • Flash off
  • Panel is now ready for clearcoat
Repair Steps