Blend into repaired panel VOC 45 Line 1. Cleaning Clean carefully with cleaner 70-45 Use wipe on, wipe off method 2. Preparation steps Tag cloth the area to be painted 3. Mixing ratio of basecoat: Basecoat (45-) 100% 45-R45 Diluter 70% 4. 45_basecoat_1.jpg Spray gun HVLP 1.4, pressure 0.8 to 1.5 bar Cover filler patch with reduced pressure until covered Keep the patch as small as possible Flash off until matt 5. Mixing blend in clear: 45-W10 100% 45-R45 Diluter 70% 6. Blend in clear Spray gun HVLP 1.4 pressure 2.0 Spray 1 wet coat until 10 cm of edges No flash off 7. Mixing blend in clear and basecoat Mix RFU blend in clear and RFU basecoat 1:1 8, Blend in of base coat Blend in the filler patch into wet blend-in clear Spray gun HVLP 1.4 pressure 0.8 to 1.5 Flash off 9. Mist coat Apply a mist coat over the repaired area Spray gun distance is 30 cm Flash off Panel is now ready for clearcoat Repair Steps Lakier bazowy/ nawierzchniowy Zacznij pracę z baslac już dziś - to się po prostu opłaca. Skontaktuj się z nami Skontaktuj się z lokalnym partnerem baslac już dziś i pracuj efektywniej. Znajdź dystrybutora w swojej okolicy