##  <a> </a> 

#  Poor hiding 

 

 

 

 

  Paint Defects

  

 

      ![TST 69.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/TST%2069.png.webp?itok=UtxAMEVR "TST 69.png")  



 

 Causes

- Color of undercoat substrate not matched to the topcoat colour
- Basecoat or topcoat over-thinned
- Paint not applied uniform
- Film build of topcoat too low

 

 

 

      ![paint defect - prevention.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/paint%20defect%20-%20prevention.png.webp?itok=lhkqUPyU "paint defect - prevention.png")  



 

 Prevention

- A uniform adapted substrate is required, especially when you apply translucent colors (e.g. 3-stage pearl effect finishes)
- Mix paint according to technical data sheets
- Use the recommended ground coats for poor-covering colours
- Ensure sufficient film thickness and respect appropriate flash-off intervals between coats

 

 

 

      ![paint defects - repair.png](https://www.baslac.com/data/sites/baslac/files/styles/ars__ratio_43__531x398/public/2024-01/paint%20defects%20-%20repair_0.png.webp?itok=eXS0Aq4P "paint defects - repair.png")  



 

 How to repair

- After drying, sand lightly and repaint

 

 

 

 

 

 

 

 



Repair Steps

[Lakier bazowy/ nawierzchniowy](/pl-emea/taxonomy/term/165)

[Lakier bezbarwny](/pl-emea/taxonomy/term/166)

[Podkład/ Szpachla](/pl-emea/taxonomy/term/172)

[Szpachla](/pl-emea/taxonomy/term/162)

[Szpachla do szlifowania](/pl-emea/taxonomy/term/163)

[Szpachla mokro na mokro](/pl-emea/taxonomy/term/164)

 

 

 

 Zacznij pracę z baslac już dziś - to się po prostu opłaca.

 

  [Skontaktuj się z nami

  ](/pl-emea/kontakt "Skontaktuj się z nami")  

 

 

 Skontaktuj się z lokalnym partnerem baslac już dziś i pracuj efektywniej.

 

  [Znajdź dystrybutora w swojej okolicy

  ](/pl-emea/dealerzy "Znajdź dystrybutora w swojej okolicy")